HS 320910
Fentin Fuskar Gini na Waje Acrylic
Fentin ginin bulo na acrylic tsantsa da styrene-acrylic don fuskar gini da aka yi wa filasta da ta kankare, fari da launukan RAL.
ƘiyasiUSD 1.10 - 2.40/ kowace kilogiramFOB Mersin / Ambarli, Turkiyya ko Guangzhou, China
Fenti na ruwa mai jure yanayi don fuskar gini da aka yi wa filasta, ta kankare da ta fibre-cement. Ajin acrylic tsantsa suna riƙe launi kuma suna jure zama gari (chalking) na tsawon lokaci a ƙarƙashin rana ta Gulf da ta wurare masu zafi; ajin styrene-acrylic su ne zaɓin farashi don yanayi mai sauƙi da kasafin kuɗin ayyuka masu matsewa. Masana'antun Turkiyya, China, UAE da Saudiyya suna gasa a wannan ciniki, Turkiyya ta fi ƙarfi a hidimar haɗa launi da lokacin shiri. Farashi a kowace kilogiram ya dogara da nau'in mai ɗaurawa, matakin TiO2, zurfin launi da kunshi. Tayin yana tabbatar da mai ɗaurawa, jerin launukan RAL, juriyar ɗaukar datti, girman kunshi da rabon kwantena bisa launi.
Kayayyaki da farashin ƙiyasi (8)
Farashin ƙiyasi a USD da aka tattara daga rahotannin kasuwa na jama'a, an sabunta a Nuwamba 2026. Farashi yana canzawa tare da kasuwannin ƙarfe, makamashi da jigila; ana sanya tabbataccen farashi, yawa da ranar isarwa a takardar kuɗi ta proforma.
Bayanan fasaha
- Mai ɗaurawa (binder)
- Acrylic tsantsa (AC) ko styrene-acrylic (SA)
- Wucewar tururin ruwa
- EN 1062-1 aji V2
- Shan ruwa
- EN 1062-1 aji W2
- Faɗin da yake rufewa
- 6-9 m2/l a kowane shafi
- Bushewa a 23°C
- Bushewar taɓawa 1 h, sake shafawa bayan 4 h